C 1

detalhe

Description

Economical low carbon steel for structural applications. Used in the cold drawn or turned condition, it is not recommended for Heat Treatment, although carbonitriding or nitriding may be applied in time.

Main applications

  • Machinery components
  • shafts and pins
  • nuts and bolts
  • threaded rod
  • rods

Delivery status

Calibrated

Hardness of the supply

  • Min: -
  • Med: -
  • Max: -
  • Composition
  • Services
  • Heat Treatments
  • Download

Profiles available

Thickness Tolerance
Round 2,5 - 130 mm EN 10278
Square 5 - 60 mm EN 10278
Rectangular 4 - 50 mm EN 10278

Chemical composition (%) 1

Min Med Max
C
0,20
Mn
1,40
P
0,040
S
0,040
Cu
0,55
N
0,012

Physical properties

Density : 7,84
10ˉ⁶m/mK
20 a 100 ⁰C 20 a 200 ⁰C 20 a 300 ⁰C 20 a 400 ⁰C 20 a 500 ⁰C 20 a 600 ⁰C 20 a 700 ⁰C
11,6 12,3 13,1 13,7 14,2 14,7 ---

Thermal Conductivity W/mk
20 ⁰C 200 ⁰C 300 ⁰C 350 ⁰C 400 ⁰C 600⁰C 700 ⁰C
15,1 --- --- --- --- --- ---

GPa
-100 ⁰C 0 ⁰C 20 ⁰C 100 ⁰C 200 ⁰C 300 ⁰C 400 ⁰C 500 ⁰C 600 ⁰C
--- --- 200 --- --- --- --- --- ---

Mechanical properties

Condition Ø Thickness Mechanical properties
Hardness Rm Rp0,2 ReH RC A Z
Hardened and tempered ≥ 5 - ≤ 10 - - - - - - - -
Drawn (+C) ≥ 5 - ≤ 10 - - - - - - - -
Ground (+SH) ≥ 5 - ≤ 10 - - - - - - - -
N/A ≥ 5 - ≤ 10 - - - - - - - -
Hardened and tempered ≤ 16 - - - - - - - -
Drawn (+C) ≤ 16 - - - - - - - -
Ground (+SH) ≤ 16 - - - - - - - -
N/A ≤ 16 - - - - - - - -
Hardened and tempered ≤ 40 - - - - - - - -
Drawn (+C) ≤ 40 - - - - - - - -
Ground (+SH) ≤ 40 - - - - - - - -
N/A ≤ 40 - - - - - - - -
Hardened and tempered ≤ 63 - - - - - - - -
Drawn (+C) ≤ 63 - - - - - - - -
Ground (+SH) ≤ 63 - - - - - - - -
N/A ≤ 63 - - - - - - - -
Hardened and tempered ≤ 100 - - - - - - - -
Drawn (+C) ≤ 100 - - - - - - - -
Ground (+SH) ≤ 100 - - - - - - - -
N/A ≤ 100 - - - - - - - -
Hardened and tempered - - - - - - - - -
Drawn (+C) - - - - - - - - -
Ground (+SH) - - - - - - - - -
N/A - - - - - - - - -
  • Composition

    Profiles available

      • Round
      • 2,5 - 130 mm
      • EN 10278
      • Square
      • 5 - 60 mm
      • EN 10278
      • Rectangular
      • 4 - 50 mm
      • EN 10278

    Chemical composition (%) 1

    Min Med Max
    C
    0,20
    Mn
    1,40
    P
    0,040
    S
    0,040
    Cu
    0,55
    N
    0,012

    Physical properties

    Density : 7,84
    10ˉ⁶m/mK
    20 a 100 ⁰C 11,6
    20 a 200 ⁰C 12,3
    20 a 300 ⁰C 13,1
    20 a 400 ⁰C 13,7
    20 a 500 ⁰C 14,2
    20 a 600 ⁰C 14,7
    20 a 700 ⁰C ---

    Thermal Conductivity W/mk
    20 ⁰C 15,1
    200 ⁰C ---
    300 ⁰C ---
    350 ⁰C ---
    400 ⁰C ---
    600⁰C ---
    700 ⁰C ---

    GPa
    -100 ⁰C ---
    0 ⁰C ---
    20 ⁰C 200
    100 ⁰C ---
    200 ⁰C ---
    300 ⁰C ---
    400 ⁰C ---
    500 ⁰C ---
    600 ⁰C ---

    Mechanical properties

    Please refer to the table in the downloads section.

  • Services
  • Heat Treatments
  • Download

Advanced Search

Hardness HB

Hardness HRC

Resistance to abrasive wear

Resistance to adhesive wear

Resistance to tempering

Resistance to heat wear

Resistance to fatigue

Compressive strength

Toughness

Ductility

Corrosion resistance

Machinability

Suitability for welding

Suitability for polishing

Thermal fatigue

Suitability for nitriding

Suitability for texture

Number of cycles (Durability)

Creep resistance

Hardenability

Find products

If you do not find the configuration you are looking for, please see Advanced Search.

Advanced Search